Common Injection Molding Defects: Flash, Sink Marks, Short Shots and Warpage

Common Injection Molding Defects: Flash, Sink Marks, Short Shots and Warpage

Most problems with molded plastic parts fall into four groups: flash, sink marks, short shots and warpage. There is rarely a single cause; the mold, material, process settings and part design all play a part. Here is what each defect looks like, why it happens and how to fix it.

1. Flash

  • What it looks like: a thin layer of extra plastic along the parting line, ejector pins or slides.
  • Common causes: insufficient clamping force, worn or poorly fitting parting surfaces, excessive injection pressure or speed, high melt temperature.
  • How to fix: check machine tonnage, repair the parting surfaces, reduce pressure and temperature.

2. Sink marks

  • What it looks like: depressions on the surface, especially over thick sections or behind ribs.
  • Common causes: thick or uneven walls, insufficient holding pressure or time, inadequate cooling.
  • How to fix: design for uniform wall thickness, core out thick areas or use ribs, increase holding pressure and cooling time.

3. Short shots

  • What it looks like: the part is incomplete, with a corner or end not filled.
  • Common causes: insufficient shot size, low melt or mold temperature, poor venting, small gates or long flow lengths.
  • How to fix: check the machine’s shot capacity, raise temperature or injection speed, improve venting, adjust gate location.

4. Warpage

  • What it looks like: the part does not sit flat, with lifted corners or twisting.
  • Common causes: uneven mold cooling, large wall thickness differences, uneven shrinkage (especially with glass-filled resins), ejecting too early.
  • How to fix: balance mold cooling, keep walls consistent, adjust gate location, extend cooling time.

Other common issues

  • Silver streaks and bubbles: often caused by moisture; hygroscopic resins such as nylon and PC must be dried.
  • Weld lines: lines where two flow fronts meet; adjust gate location or raise temperature.
  • Stress whitening: white marks during ejection; adjust ejection or draft angles.

Many defects can be prevented before tooling by reviewing wall thickness, draft angles and gate location.

Struggling with flash, sink marks or warpage? Send us your samples or drawings, and Chien Chen will review the mold, material and process settings with you. Request a quote.